Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 547 MPa @Strain 0.200 %, Temperature 600 °C |
79300 psi @Strain 0.200 %, Temperature 1110 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed, Age-hardened Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |
|||
Tensile Strength, Yield | 547 MPa @Temperature 71.0 °C |
79300 psi @Temperature 160 °F |
|
Hexcel® HexPly® F155 Epoxy Resin, K285 Kevlar Fabric Information provided by HexCel |
|||
Tensile Strength, Yield | 547 MPa @Strain 0.200 %, Temperature 600 °C |
79300 psi @Strain 0.200 %, Temperature 1110 °F |
|
Special Metals NIMONIC® alloy 91 Ni-Cr-Co Alloy NIMONIC® alloy 91 is a wrought nickel-chromium-cobalt based alloy strengthened by additions of aluminum and titanium.This alloy is a modification of NIMONIC alloy 90, but has an increased chromium .. |