Tensile Strength, Yield 376 MPa

@Thickness 12.7 mm,
Temperature 427 °C
54500 psi

@Thickness 0.500 in,
Temperature 801 °F
0.2% Offset
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Tensile Strength, Yield 376 MPa

@Strain 0.200 %,
Temperature 25.0 °C
54500 psi

@Strain 0.200 %,
Temperature 77.0 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Tensile Strength, Yield 376 MPa

@Thickness 3.20 mm,
Temperature 20.0 °C
54500 psi

@Thickness 0.126 in,
Temperature 68.0 °F
0.2% offset
Haynes Hastelloy® C-4 alloy, sheet, aged 100 hours at 899°C
Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T..