Polymer Property : Tensile Strength, Yield = 525 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 525 MPa

@Thickness 50.8 - 152 mm
76100 psi

@Thickness 2.00 - 6.00 in
at center (L/T direction)
Alcoa QC-10® Aluminum Mold Alloy
Specifically designed for high production injection and blow mold applications, QC-10 offers outstanding strength, stability, and durability. Its improved alloy composition provides outstanding, 1"-..
Tensile Strength, Yield 525 MPa

@Strain 0.200 %,
Thickness 6.50 - 12.0 mm
76100 psi

@Strain 0.200 %,
Thickness 0.256 - 0.472 in
Typical Strength
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..
Tensile Strength, Yield 525 MPa

@Strain 0.200 %,
Thickness 12.0 - 25.0 mm
76100 psi

@Strain 0.200 %,
Thickness 0.472 - 0.984 in
Typical Strength
Constellium Fortal® Aluminum Alloy
Fortal® plates are optimized to provide high mechanical strength, combined with good shape stability and excellent machinability. Typical applications include sheet forming tools, base plates for m..