Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 359 MPa @Temperature 23.9 °C |
52000 psi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D638 Type 1 |
Park Electrochemical Nelcote® P-650M Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-650M is a polyester resin system suitable for coating on any MIL-C-9084. P-650M has good electrical and mechanical properties and has been used in a wide variety of applications, includi.. |
|||
Tensile Strength, Yield | 359 MPa @Temperature 149 °C |
52000 psi @Temperature 300 °F |
0° Direction, Dry; ASTM D638 |
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 7781 E-Glass Reinforced Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp.. |