Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 347 MPa @Thickness 25.4 mm, Temperature 93.0 °C |
50300 psi @Thickness 1.00 in, Temperature 199 °F |
0.2% Offset |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |