Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 502 MPa @Treatment Temp. 502 °C, Time 3.60e+6 sec |
72800 psi @Treatment Temp. 936 °F, Time 1000 hour |
0.2%. Room temp test after thermal exposure |
Haynes 282® Nickel Alloy Sheet, Gamma-Prime Strengthened Excellent High Temperature Strength HAYNES® 282® alloy is a wrought, gamma-prime strengthened superalloy developed for high temperature structural applications, especially those in aero and land-b.. |