Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 5.50 MPa @Strain 50.0 % |
798 psi @Strain 50.0 % |
ASTM D412 |
GRECO ISOTHANE 1190A Poly(adipate)ester TPUÂ Resin ISOTHANE 1100 series products are transparent grade, polyester poly(adipate)ester based thermoplastic polyurethanes. They exhibit good toughness, solvent resistance, easy processing, and high transp.. |
|||
Tensile Strength, Yield | 5.50 MPa @Strain 100 % |
798 psi @Strain 100 % |
ASTM D412 |
GRECO ISOTHANE 3080A Polyether TPU Resin ISOTHANE 3000 Series products are polyether based thermoplastic polyurethanes. They exhibit excellent hydrolytic resistance, fungus resistance, and low temperature performance properties. These prod.. |
|||
Tensile Strength, Yield | 5.50 MPa @Strain 100 % |
798 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® C-80A Polyester Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan C series of products are polyester-based thermoplastic polyurethanes that exhibit very good hydrolytic stability. They also exhibit excellen.. |
|||
Tensile Strength, Yield | 5.50 MPa @Strain 100 % |
798 psi @Strain 100 % |
ASTM D-412 |
BASF Elastollan® 1180A Polyether Type Polyurethane Elastomer Processed by extrusion or injection molding. Elastollan ® 1100 series products are FDA Sec. 177.2600 compliant. Elastollan 1100 series of products are polyether-based thermoplastic polyurethanes... |