Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 34.3 MPa @Strain 300 % |
4980 psi @Strain 300 % |
ASTM D412 |
SK Chemicals SKYTHANE® 198A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 34.3 MPa @Thickness 3.20 mm |
4980 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |
|||
Tensile Strength, Yield | 34.3 MPa @Thickness 3.20 mm |
4980 psi @Thickness 0.126 in |
Type I, 5 mm/min; ASTM D638 |
Bhansali Engineering Abstron BL60 Impact modifier for PVC Impact modifier for PVC, White powderInformation provided by Bhansali |