Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 498 MPa @Strain 0.200 %, Time 3.60e+6 sec |
72200 psi @Strain 0.200 %, Time 1000 hour |
Room Temperature properties after Isothermal Exposure |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |
|||
Tensile Strength, Yield | 498 MPa @Strain 0.200 %, Treatment Temp. 650 °C |
72200 psi @Strain 0.200 %, Treatment Temp. 1200 °F |
Room Temperature properties after Isothermal Exposure |
Special Metals INCOLOY® alloy 803 Fe-Ni-Cr Alloy INCOLOY® alloy 803 (UNS S35045), an iron-nickel-chromium alloy, is designed for use in petrochemical, chemical and thermal processing applications. The nickel and chromium contents of alloy 803 ar.. |