Tensile Strength, Yield 3223 MPa

@Strain 0.200 %,
Temperature 760 °C
467500 psi

@Strain 0.200 %,
Temperature 1400 °F
AMS 5879
Haynes 625SQ® Nickel Alloy Sheet
Haynes 625SQ alloy is a solid-solution strengthened superalloy. It is a modification of Haynes 625 alloy designed to enhance resistance to fatigue at temperatures up to approximately 1200°F (649Â..