Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 463 MPa @Thickness 12.7 mm, Temperature 93.0 °C |
67200 psi @Thickness 0.500 in, Temperature 199 °F |
0.2% Offset |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Shielded Metal Arc Welded (SMAW) Plate HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |
|||
Tensile Strength, Yield | 463 MPa @Strain 0.200 % |
67100 psi @Strain 0.200 % |
11-15in thick |
Clinton Aluminum Alumold 1-500 Forged Alumold 1-500 Forged is a high quality, high strength aluminum alloy intended for the plastic forming industry and for other tooling applications. With its high strength and surface hardness it is .. |
|||
Tensile Strength, Yield | 463 MPa @Strain 0.200 % |
67100 psi @Strain 0.200 % |
15-17in thick |
Clinton Aluminum Alumold 1-500 Forged Alumold 1-500 Forged is a high quality, high strength aluminum alloy intended for the plastic forming industry and for other tooling applications. With its high strength and surface hardness it is .. |
|||
Tensile Strength, Yield | 463 MPa @Strain 0.200 % |
67100 psi @Strain 0.200 % |
7-11in thick |
Clinton Aluminum Alumold 1-500 Forged Alumold 1-500 Forged is a high quality, high strength aluminum alloy intended for the plastic forming industry and for other tooling applications. With its high strength and surface hardness it is .. |