Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 318 MPa @Temperature 200 °C |
>= 46100 psi @Temperature 392 °F |
|
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6 High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |
|||
Tensile Strength, Yield | 318 MPa @Thickness 12.7 mm, Temperature 25.0 °C |
46100 psi @Thickness 0.500 in, Temperature 77.0 °F |
0.2% Offset |
Haynes Hastelloy® G-35® Nickel Alloy Plate, Annealed at 2075°F (1135°C) Known for its corrosion performance, HASTELLOY® G-35® alloy was designed to resist “wet process†phosphoric acid, which is widely used in the production of fertilizers. Tests indicat.. |