Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 309.9 MPa @Strain 0.200 % |
44950 psi @Strain 0.200 % |
as cast |
Wieland BioPortadur Casting Alloy Gold casting alloyApplications: inlays/onlays, crowns, short span bridges, long span bridges, telescopic and milling works, removable partials, acrylic veneeringDental |