Polymer Property : Tensile Strength, Yield = 44.6 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 44.6 MPa

@Strain 0.200 %
6470 psi

@Strain 0.200 %
Transverse to Sheet Rolling Direction, Tensile Hardness Test (ASTM E8, E694, E18, A370)
AK Steel 430 ULTRA FORM® Stainless Steel
430 ULTRA FORM® Stainless Steel was developed as a more formable version of Type 430 stainless steel. It is particularly suited for parts requiring more complex shapes. 430 ULTRA FORM Stainless Ste..