Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 439 MPa @Strain 0.200 %, Temperature 25.0 °C |
63700 psi @Strain 0.200 %, Temperature 77.0 °F |
|
Haynes Hastelloy® C-22HS™ Nickel Alloy Sheet, Cold-rolled, Solution Annealed Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou.. |