Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 434 MPa @Thickness 1.45 mm, Temperature 20.0 °C |
62900 psi @Thickness 0.0571 in, Temperature 68.0 °F |
0.2% offset |
Haynes Hastelloy® S alloy, flat products Nickel-based, high temperature alloy. Excellent thermal stability, low thermal expansion, excellent oxidation resistance to 1093°C, good high temperature and thermal fatigue strength. Application.. |
|||
Tensile Strength, Yield | 434 MPa @Strain 0.200 % |
62900 psi @Strain 0.200 % |
Sheet |
Special Metals INCONEL® alloy 22 Austenitic Alloy INCONEL® alloy 22 (UNS N06022; W.Nr. 2.4602; NiCr21Mo14W) is a fully austenitic advanced corrosion-resistant alloy that offers resistance to both aqueous corrosion and attack at elevated temperat.. |
|||
Tensile Strength, Yield | 434 MPa @Thickness 12.7 mm, Temperature 20.0 °C |
62900 psi @Thickness 0.500 in, Temperature 68.0 °F |
0.2% offset |
Haynes Hastelloy® C-22® alloy, transverse, GTAW short arc weldment, plate HASTELLOY® C-22® alloy is a nickel-chromium-molybdenum-tungsten alloy with excellent overall corrosion resistance compared to other Ni-Cr-Mo alloys, including HASTELLOY C-276 and C-4 alloys and al.. |
|||
Tensile Strength, Yield | 434 MPa @Strain 0.200 %, Thickness 25.4 mm |
62900 psi @Strain 0.200 %, Thickness 1.00 in |
as welded |
Haynes Hastelloy® C-22HS™ Nickel Alloy Synergic Gas Metal Arc Welded (GMAW) Plate Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately doubl.. |