Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 429 MPa @Temperature 20.0 °C |
>= 62200 psi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S693 Aluminum Alloy, AlCu5Ti, Condition T6 High stiffness and elongation at rupture. Property data for Condition T6 (Quench in water at RT).Information provided by PEAK Werkstoff GmbH |