Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 4.22 - 4.41 MPa @Strain 10.0 % |
612 - 640 psi @Strain 10.0 % |
ASTM D638 |
Samyang Triel® 5400 Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |
|||
Tensile Strength, Yield | 4.22 - 4.41 MPa @Strain 10.0 % |
612 - 640 psi @Strain 10.0 % |
ASTM D638 |
Samyang Triel® 5407EF Thermoplastic Polyether Ester Elastomer TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor r.. |