Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 395 MPa @Strain 1.00 % |
57300 psi @Strain 1.00 % |
Outokumpu Typical,Cold Rolled Strip/Sheet; EN 10002-1 |
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
Tensile Strength, Yield | 395 MPa @Strain 0.200 %, Thickness 38.1 - 76.2 mm |
57300 psi @Strain 0.200 %, Thickness 1.50 - 3.00 in |
Typical Strength |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |
|||
Tensile Strength, Yield | 395 MPa @Strain 0.200 %, Thickness 76.2 - 127 mm |
57300 psi @Strain 0.200 %, Thickness 3.00 - 5.00 in |
Typical Strength |
Constellium Alumold® 400 Aluminum The Alumold®-400 alloy has been optimized to provide good shape stability and high strength properties throughout the plate thickness. Typical applications include blow moulds, thermoforming moulds.. |