Mechanical Properties Metric English Comments
Tensile Strength, Yield 391 MPa

@Diameter 12.7 mm,
Temperature 260 °C
56700 psi

@Diameter 0.500 in,
Temperature 500 °F
0.2% offset
Haynes Hastelloy® C-2000® Nickel Alloy Gas Tungsten Arc Welded (GTAW) All Weld Cruciform
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..
Tensile Strength, Yield 391 MPa

@Thickness 12.7 mm,
Temperature 204 °C
56700 psi

@Thickness 0.500 in,
Temperature 399 °F
0.2% Offset
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Tensile Strength, Yield 391 MPa

@Temperature 25.0 °C
56700 psi

@Temperature 77.0 °F
Open Hole Tensile, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, SGP196-PW Fiber
Information provided by HexCel
Tensile Strength, Yield 391 MPa

@Temperature 93.0 °C
56700 psi

@Temperature 199 °F
ATI Wah Chang Zircadyne® Alloy Zr 705
Zircadyne 705 is zirconium alloyed with niobium to increase its strength and improve its formability. Alloy exhibits good ductility even at cryogenic temperatures and strength comparable with other ..