Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 26.4 MPa @Strain 1.00 % |
3830 psi @Strain 1.00 % |
ASTM D95 |
Daelim H&L Plavis N Aromatic Polyimide, Non-Filled, Machined Parts Superior chemical property, very high radiation resistance, electrical and thermal property, low outgassing and superior physical propertyInformation provided by Daelim H&L |