Polymer Property : Tensile Strength, Yield = 38100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 263 MPa

@Strain 0.200 %,
Temperature 300 °C
38100 psi

@Strain 0.200 %,
Temperature 572 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Tensile Strength, Yield 263 MPa

@Temperature 177 °C
38100 psi

@Temperature 351 °F
Hexcel® HexPly® F263 Epoxy Resin, 120 Glass Fabric
Hexcel designation: 120-38"-F263; Fiber: 450-1/2Information provided by HexCel
Tensile Strength, Yield 263 MPa

@Strain 0.200 %
38100 psi

@Strain 0.200 %
Annealed
AK Steel 439 ULTRA FORM® Stainless Steel
AK Steel 439 ULTRA FORM™ was developed for applications requiring oxidation and corrosion resistance superior to Type 409 as well as superior formability to AK Steel 439 Stainless Steel. As a resul..