Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 0.262 MPa @Temperature 25.0 °C |
38.0 psi @Temperature 77.0 °F |
|
Unifrax Fiberfrax® Fiberwall® 601 Inconel Systems Hardware The Fiberwall® systems family of anchoring hardware and accessory components provides an array of attachment options to cover a broad range of lining system designs and application requirements. I.. |
|||
Tensile Strength, Yield | 0.262 MPa @Temperature 25.0 °C |
38.0 psi @Temperature 77.0 °F |
|
Unifrax Fiberfrax® Fiberwall® 304 SS Systems Hardware The Fiberwall® systems family of anchoring hardware and accessory components provides an array of attachment options to cover a broad range of lining system designs and application requirements. I.. |
|||
Tensile Strength, Yield | 0.262 MPa @Temperature 25.0 °C |
38.0 psi @Temperature 77.0 °F |
|
Unifrax Fiberfrax® Fiberwall® 330 SS Systems Hardware The Fiberwall® systems family of anchoring hardware and accessory components provides an array of attachment options to cover a broad range of lining system designs and application requirements. I.. |
|||
Tensile Strength, Yield | 0.262 MPa @Temperature 25.0 °C |
38.0 psi @Temperature 77.0 °F |
|
Unifrax Fiberfrax® Fiberwall® 310 SS Systems Hardware The Fiberwall® systems family of anchoring hardware and accessory components provides an array of attachment options to cover a broad range of lining system designs and application requirements. I.. |
|||
Tensile Strength, Yield | 0.262 MPa @Strain 50.0 % |
38.0 psi @Strain 50.0 % |
250 mm/min; ASTM D412A |
PolyOne Elastamax™ XL 0141-66 Styrene Butadiene Block Copolymer (SBC)
(discontinued **) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |