Mechanical Properties Metric English Comments
Tensile Strength, Yield 2570 MPa

@Temperature -55.0 °C
373000 psi

@Temperature -67.0 °F
0°, Dry
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber
Information provided by HexCel