Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 366 MPa @Strain 0.200 %, Thickness 7.90 - 50.8 mm |
53100 psi @Strain 0.200 %, Thickness 0.311 - 2.00 in |
Typical Strength |
Constellium Alumold® 350 Aluminum Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti.. |
|||
Tensile Strength, Yield | 366 MPa @Strain 0.200 %, Thickness 50.8 - 76.2 mm |
53100 psi @Strain 0.200 %, Thickness 2.00 - 3.00 in |
Typical Strength |
Constellium Alumold® 350 Aluminum Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti.. |
|||
Tensile Strength, Yield | 366 MPa @Strain 0.200 %, Thickness 76.2 - 101.6 mm |
53100 psi @Strain 0.200 %, Thickness 3.00 - 4.000 in |
Typical Strength |
Constellium Alumold® 350 Aluminum Alumold-350® has been specifically developed to achieve the best combination of strength at low and high temperatures, together with a good shape stability and machinability. Alumold-350® is parti.. |