Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 303 - 359 MPa @Strain 0.200 % |
43900 - 52100 psi @Strain 0.200 % |
Typical |
AK Steel 18 Cr-Cb™ Ferritic Stainless steel AK Steel 18 Cr-Cb™ provides a more effective solution than Type 409 to many automotive exhaust applications, due to its higher oxidation resistance, improved creep resistance and moderate formabili.. |