Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 243 MPa @Strain 0.200 %, Temperature 316 °C |
35200 psi @Strain 0.200 %, Temperature 601 °F |
|
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C) Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h.. |