Polymer Property : Tensile Strength, Yield = 351 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 351 MPa

@Thickness 12.7 mm,
Temperature 316 °C
50900 psi

@Thickness 0.500 in,
Temperature 601 °F
0.2% Offset
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Gas Tungsten Arc Welded (GTAW) Plate
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing..
Tensile Strength, Yield 351 MPa

@Strain 0.200 %
50900 psi

@Strain 0.200 %
ASTM E8
ATI Allegheny Ludlum 309S Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..