Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 349 MPa @Temperature 132 °C |
50600 psi @Temperature 270 °F |
Dry |
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric Hexcel designation: 285-38"-F161; Fiber: Kev. 49 1140Information provided by HexCel |