Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 342 MPa @Strain 0.200 %, Temperature 25.0 °C |
49600 psi @Strain 0.200 %, Temperature 77.0 °F |
|
Haynes HR-224® Nickel Alloy Alloy with excellent oxidation resistance and improved fabricability and weldability compared to HAYNES® 214® alloy. This Ni–27.5Fe–20Cr–3.8Al alloy achieves superior oxidation .. |
|||
Tensile Strength, Yield | 342 MPa @Temperature 177 °C |
49600 psi @Temperature 351 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with Fiberglass 7781 fabric reinforcement Laminate Physicals: 53% Fiber volume, 29% Resin content, 0.5% VoidsInformation provided by HexCel |