Tensile Strength, Yield 225.5 MPa

@Thickness 2.00 mm,
Temperature 427 °C
32710 psi

@Thickness 0.0787 in,
Temperature 801 °F
0.2% offset
Haynes Hastelloy® C-276 alloy, solution heat treated flat products
Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn'..
Tensile Strength, Yield 225.5 MPa

@Thickness 4.80 - 25.4 mm,
Temperature 427 °C
32710 psi

@Thickness 0.189 - 1.00 in,
Temperature 801 °F
0.2% offset
Haynes Hastelloy® C-276 alloy, solution heat treated flat products
Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn'..