Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 223 MPa

@Temperature 20.0 °C
>= 32300 psi

@Temperature 68.0 °F
PEAK Werkstoff DISPAL S263 Aluminum Alloy, AlSi25Cu3Fe3Ni3MgCoTi, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Tensile Strength, Yield 223 MPa

@Strain 0.200 %,
Temperature 600 °C
32300 psi

@Strain 0.200 %,
Temperature 1110 °F
Haynes Hastelloy® C-22HS™ Nickel Alloy Plate and Bar, Hot-rolled, Solution Annealed
Outstanding Corrosion Resistance, High Strength HASTELLOY® C-22HSTM alloy is corrosion-resistant, nickel-chromium-molybdenum alloy which can be heat treated to obtain a strength approximately dou..
Tensile Strength, Yield 223 MPa

@Strain 0.200 %,
Temperature 482 °C
32300 psi

@Strain 0.200 %,
Temperature 900 °F
Haynes Hastelloy® C-2000® Bar, Annealed at 2100°F (1149°C)
Nickel-chromium-molybdenum (Ni-Cr-Mo) C-type alloys have a long history of use in the Chemical Process Industries and are known for their versatility. Not only do they resist all acids (especially h..