Polymer Property : Tensile Strength, Yield = 3.72 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.72 MPa

@Strain 300 %
540 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL-0153-56 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)
A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco..
Tensile Strength, Yield 3.72 MPa

@Strain 300 %
540 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL-0153-79 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)
A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco..