Polymer Property : Tensile Strength, Yield = 3.53 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 3.53 MPa

@Strain 100 %
512 psi

@Strain 100 %
ASTM D412
SK Chemicals SKYTHANE® 875A T series Polyurethane
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr..
Tensile Strength, Yield 3.53 - 3.73 MPa

@Strain 10.0 %
512 - 540 psi

@Strain 10.0 %
ASTM D638
Samyang Triel® 5300 Thermoplastic Polyether Ester Elastomer
TRIEL® resins offer superior mechanical properties, elasticities, heat and chemical resistance, which allow it to be widely used for electric/electronic equipments, automotive parts and outdoor rec..