Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 199 MPa @Strain 1.00 %, Temperature 100 °C |
28900 psi @Strain 1.00 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Tensile Strength, Yield | 199 MPa @Strain 1.00 %, Temperature 100 °C |
28900 psi @Strain 1.00 %, Temperature 212 °F |
EN min.; EN 10002-5 |
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |