Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength, Yield = 285 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield >= 285 MPa

@Strain 0.200 %
>= 41300 psi

@Strain 0.200 %
Industeel CLC 17.13.5 LN Modified 317LN Mo 4% Austenitic Stainless Steel
Description: CLC 17-13-5LN (317LNM) is a Nitrogen alloyed austenitic stainless steel with a high Molybdenum addition (=4%). Alloy CLC 17-13-5LN (317LNM) exhibits austenitic microstructure free of de..
Tensile Strength, Yield 285 MPa

@Strain 0.200 %
41300 psi

@Strain 0.200 %
Typical after Solution Annealing
Industeel SIRIUS 314 25% Cr - 1.8% Si Heat Resistant Stainless Steel
Description: CLI SIRIUS 314 grade is a fully austenitic stainless steel containing 25% Cr, 20% Ni and 1.8% Si. The alloy is designed for high temperature corrosion resistance applications even in se..
Tensile Strength, Yield 285 MPa

@Strain 0.200 %,
Thickness 4.00 - 8.00 mm
41300 psi

@Strain 0.200 %,
Thickness 0.157 - 0.315 in
Typical Strength; Standard EN 485-2
Constellium PLAN 6061 Aluminum Rolled Plate
Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
Tensile Strength, Yield 285 MPa

@Strain 0.200 %,
Thickness 60.0 - 150 mm
41300 psi

@Strain 0.200 %,
Thickness 2.36 - 5.91 in
Typical Strength; Standard EN 485-2
Constellium PLAN 6061 Aluminum Rolled Plate
Rolled plates in 6061 PLAN are optimized for minimum residual stress and improved dimensional tolerances. 6061 PLAN is mainly used for medium stressed mechanical components, manufactured by intensiv..
Tensile Strength, Yield 285 MPa

@Strain 0.200 %,
Thickness 60.0 - 150 mm
41300 psi

@Strain 0.200 %,
Thickness 2.36 - 5.91 in
Typical Strength
Constellium ALPLAN® 6061 Rolled Precision Aluminum Plate, Milled Both Sides
Precision plates in ALPLAN® 6061 are milled on both sides and have a very low level of residual stress, thus avoiding excessive deformation during machining. Thanks to its very good dimensional sta..