Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1930 MPa @Strain 0.200 %, Temperature 482 °C |
280000 psi @Strain 0.200 %, Temperature 900 °F |
Solution Annealed Plus Aged, AC |
Special Metals UDIMAR® alloy 300 Fe-Ni Maraging Steel UDIMAR® alloy 300 (UNS K93120) is an age-hardenable (maraging) iron-nickel steel combining ultra-high strength, toughness and resistance to crack propagation. The alloy is well suited to applica.. |
|||
Tensile Strength, Yield | 1930 MPa @Strain 0.200 %, Time 10800 sec |
280000 psi @Strain 0.200 %, Time 3.00 hour |
Solution Annealed Plus Aged, AC |
Special Metals UDIMAR® alloy 300 Fe-Ni Maraging Steel UDIMAR® alloy 300 (UNS K93120) is an age-hardenable (maraging) iron-nickel steel combining ultra-high strength, toughness and resistance to crack propagation. The alloy is well suited to applica.. |