Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 28.1 MPa @Strain 1.00 % |
4080 psi @Strain 1.00 % |
ASTM D95 |
Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Direct Formed
(Unverified Data**) Information provided by Daelim H&L |