Mechanical Properties Metric English Comments
Tensile Strength, Yield 188 MPa

@Temperature 427 °C
27300 psi

@Temperature 801 °F
ASTM E8
ATI Allegheny Ludlum 310 Austenitic Stainless Steel
Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo..