Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 272 MPa @Strain 0.200 %, Temperature 22.0 °C |
39500 psi @Strain 0.200 %, Temperature 71.6 °F |
Hot-Rolled Plate, Solution-Annealed |
Special Metals INCOLOY® alloy 890 Ni-Cr-Fe Superalloy INCOLOY® alloy 890 (UNS N08890) is the latest addition to the INCOLOY alloy family of heat resistant alloys. Alloy 890 joins the existing INCOLOY products in offering high strength along with ex.. |
|||
Tensile Strength, Yield | 272 MPa @Temperature 149 °C |
39500 psi @Temperature 300 °F |
|
ATI Wah Chang Zircadyne® Alloy Zr 705 Zircadyne 705 is zirconium alloyed with niobium to increase its strength and improve its formability. Alloy exhibits good ductility even at cryogenic temperatures and strength comparable with other .. |
|||
Tensile Strength, Yield | 272 MPa @Thickness 9.50 mm, Temperature 204 °C |
39500 psi @Thickness 0.374 in, Temperature 399 °F |
0.2% offset |
Haynes Hastelloy® C-4 alloy, sheet, aged 100 hours at 899°C Nickel-chromium-molybdenum alloy with outstanding high-temperature stability as evidenced by high ductility and corrosion resistance even after aging in the 1200 to 1900°F (649 to 1038°C) range. T.. |