Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 18.6 MPa @Strain 100 % |
2700 psi @Strain 100 % |
ASTM D412 |
SK Chemicals SKYTHANE® 155D R series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 18.6 MPa @Strain 300 % |
2700 psi @Strain 300 % |
ASTM D412 |
SK Chemicals SKYTHANE® 190A R series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 18.6 MPa @Strain 100 % |
2700 psi @Strain 100 % |
ASTM D412 |
SK Chemicals SKYTHANE® 198A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 18.6 MPa @Strain 10.0 % |
2700 psi @Strain 10.0 % |
ASTM D638 |
Samyang Triel® 5600 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5600 is an extrusion grade.Information provided by Samyang. |
|||
Tensile Strength, Yield | 18.6 MPa @Strain 300 % |
2700 psi @Strain 300 % |
ASTM D412 |
SK Chemicals SKYTHANE® 190A S series Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Tensile Strength, Yield | 18.6 MPa @Strain 5.00 % |
2700 psi @Strain 5.00 % |
ASTM D638 |
Samyang Triel® 5650 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5650 is an extrusion grade.Information provided by Samyang. |