Polymer Property : Tensile Strength, Yield = 268 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 268 MPa

@Temperature 93.0 °C
38800 psi

@Temperature 199 °F
ATI Wah Chang Zircadyne® Alloy Zr 702
Zircadyne 702 is commercially pure zirconium. Alloy exhibits good ductility even at cryogenic temperatures and good strength comparable with other common engineering alloys.Information provided by A..
Tensile Strength, Yield 268 MPa

@Thickness 19.1 mm,
Temperature 204 °C
38900 psi

@Thickness 0.752 in,
Temperature 399 °F
0.2% Offset
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Plate, Hot Rolled and Solution Annealed
HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing spe..