Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 180 MPa @Strain 1.00 %, Temperature 300 °C |
26100 psi @Strain 1.00 %, Temperature 572 °F |
EN min.; EN 10002-5 |
Outokumpu 153MA™ High Temperature Austenitic Stainless Steel Variant of 1.4301 with increased silicon and nitrogen contents and microalloyed with rare earth metals (REM). This raises the max service temperature in dry air to 1000°C.Applications: Heat and cr.. |
|||
Tensile Strength, Yield | 180 MPa @Strain 1.00 %, Temperature 500 °C |
26100 psi @Strain 1.00 %, Temperature 932 °F |
EN min.; EN 10002-5 |
Outokumpu 253MA® High Temperature Austenitic Stainless Steel Variant of 1.4828 with increased nitrogen content and has been microalloyed with rare earth metals (REM). The most suitable temperature range is 850-1100°C, because structural changes when used be.. |
|||
Tensile Strength, Yield | >= 180 MPa @Temperature 20.0 °C |
>= 26100 psi @Temperature 68.0 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Tensile Strength, Yield | 180 MPa @Temperature 23.0 °C |
26100 psi @Temperature 73.4 °F |
|
Crucible Compaction Metals Rene 95 Nickel Based Superalloy P/M Rene 95 is one of the highest strength alloys available for service in the range of 800°F to 1200°F (425°C to 650°C). The alloy also provides excellent high temperature creep resistance and.. |