Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 252 MPa @Temperature 150 °C |
>= 36500 psi @Temperature 302 °F |
|
PEAK Werkstoff DISPAL S542 Aluminum Alloy, AlMg6Mn4SiTiZrCo, Condition F Information provided by PEAK Werkstoff GmbH |
|||
Tensile Strength, Yield | 252 MPa @Thickness 25.4 mm, Temperature 371 °C |
36500 psi @Thickness 1.00 in, Temperature 700 °F |
0.2% Offset |
Haynes Hastelloy® Hybrid-BC1® Nickel Alloy Bar, Hot Rolled and Solution Annealed HASTELLOY® HYBRID-BC1® alloy possesses much higher resistance to hydrochloric and sulfuric acids than the nickel-chromium-molybdenum (C-type) alloys, and can tolerate the presence of oxidizing.. |