Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 2340 MPa @Temperature 23.9 °C |
340000 psi @Temperature 75.0 °F |
0° Direction, Dry; ASTM D3039 |
Park Electrochemical Nelcote® E-718 Epoxy Prepreg, T-700 24K Uni-Tape Reinforced Nelcote® E-718 is a modified epoxy resin system. E-718 is designed to provide excellent mechanical properties at low cure pressures.Key Features and Benefits:Good low pressure consolidationExcellen.. |
|||
Tensile Strength, Yield | 2340 MPa @Temperature 23.9 °C |
340000 psi @Temperature 75.0 °F |
0° Direction, Dry, 365° Autoclave Cured; ASTM D3039 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, IM7 Unitape Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |