Mechanical Properties Metric English Comments
Tensile Strength, Yield 233.1 MPa

@Thickness 1.60 - 4.70 mm,
Temperature 538 °C
33810 psi

@Thickness 0.0630 - 0.185 in,
Temperature 1000 °F
0.2% offset
Haynes Hastelloy® C-276 alloy, solution heat treated flat products
Hastelloy® C-276 alloy is a nickel-molybdenum-chromium wrought alloy that is a versatile corrosion-resistant alloy. C-276 alloy is an improved wrought version of alloy C in that it usually doesn'..