Mechanical Properties Metric English Comments
Tensile Strength, Yield 158 MPa

@Strain 1.00 %,
Temperature 500 °C
22900 psi

@Strain 1.00 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4406 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 158 MPa

@Strain 1.00 %,
Temperature 500 °C
22900 psi

@Strain 1.00 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms.
Tensile Strength, Yield 158 MPa

@Strain 1.00 %,
Temperature 500 °C
22900 psi

@Strain 1.00 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel
Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,..