Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1350 MPa @Temperature 93.3 °C |
196000 psi @Temperature 200 °F |
|
International Mold Steel DH21 Die Cast & Forging Steel DH21 is for aluminum die cast dies.Information provided by International Mold Steel |