Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 1270 MPa @Strain 0.200 % |
184000 psi @Strain 0.200 % |
hardness of 45 HRC |
Bohler-Uddeholm UDDEHOLM QRO® 90 SUPREME Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelQRO® 90 SUPREME is a premium hot work die steel with high hot yield strength and very good temper resistance. Especially suited for die casting of aluminum.. |