Polymer Property : Tensile Strength, Yield = 181 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 181 MPa

@Strain 1.00 %,
Temperature 100 °C
26300 psi

@Strain 1.00 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Tensile Strength, Yield 181 MPa

@Strain 1.00 %,
Temperature 100 °C
26300 psi

@Strain 1.00 %,
Temperature 212 °F
EN min.; EN 10002-5
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Tensile Strength, Yield 181 MPa

@Strain 1.00 %,
Temperature 200 °C
26300 psi

@Strain 1.00 %,
Temperature 392 °F
EN min.; EN 10002-5
Outokumpu 4878 High Temperature Austenitic Stainless Steel
Heat-resistant variant of 1.4541, with a slightly higher max carbon content. Recommended max service temperature for this steel in dry air is 800°C. Applications: Heat and creep resistance. For ..